Stability of layered coatings with outer layer made of ceramics
From MaRDI portal
Publication:741025
DOI10.1007/S10778-012-0505-2zbMATH Open1295.74034OpenAlexW1968555417MaRDI QIDQ741025FDOQ741025
Authors: D. Kharzeev
Publication date: 10 September 2014
Published in: International Applied Mechanics (Search for Journal in Brave)
Full work available at URL: https://doi.org/10.1007/s10778-012-0505-2
Recommendations
- Stability of layered coatings under biaxial thermomechanical loading
- scientific article; zbMATH DE number 1851178
- scientific article; zbMATH DE number 1800505
- scientific article; zbMATH DE number 3956618
- scientific article; zbMATH DE number 1523837
- scientific article; zbMATH DE number 1800491
- scientific article; zbMATH DE number 1524005
- Studies on ceramic coatings. Deduction of mechanical and thermal properties from the microstructure of the material
- Suppression of edge cracking in layered ceramic composites by edge coating
- Stability of a two-layer blown film coextrusion
Classical linear elasticity (74B05) Composite and mixture properties (74E30) Thermal effects in solid mechanics (74F05) Bifurcation and buckling (74G60)
Cites Work
- Establishing foundations of the mechanics of nanocomposites (review)
- Principles of the continual theory of plastic fracture of unidirectional fiber composite materials with a metallic matrix under compression
- Stress-strain state of a material under forces acting along a periodic set of coaxial mode II penny-shaped cracks
- Stability of layered materials with zero in-plane strains
- Stability of layered coatings under biaxial thermomechanical loading
- Surface instability of a layered medium connected to a uniform half-space
- Three-dimensional stability theory of deformable bodies surface instability
- Influence of surface load on stability of laminar bodies
Cited In (5)
- Studies on ceramic coatings. Deduction of mechanical and thermal properties from the microstructure of the material
- Title not available (Why is that?)
- Suppression of edge cracking in layered ceramic composites by edge coating
- Stability of layered materials with zero in-plane strains
- Stability of layered coatings under biaxial thermomechanical loading
This page was built for publication: Stability of layered coatings with outer layer made of ceramics
Report a bug (only for logged in users!)Click here to report a bug for this page (MaRDI item Q741025)